● Nitriding (e.g., ion nitriding): Raises surface hardness (HV ≥ 1000) and corrosion resistance; suitable for high temperature TIPS and chlorinated media; good for PSf/PES dopes. Less resistant to fluorinated solvents; hydrophobicity moderate; hang-up reduction less than DLC; may slightly increase roughness.
● General principle: For strong solvents (e.g., DMF), prefer DLC; for high temperature/pressure, prefer nitriding. Always test coating compatibility to avoid chemical failure.
● Material-first: Prefer SUS304/316L; only consider coatings for extreme conditions (high solids/high wear) after long-term validation.