loading

Leading Hollow Fiber Membrane Spinning Machine and Spinneret Manufacturer - Trustech

Why do hollow fiber spinnerets clog easily?

2025-12-03
● Particulates or incomplete dissolution: Solids and gel particles block orifices.

● Excessive viscosity: Slow flow increases deposition; residual dope solidifies upon stops.

● Untimely/insufficient cleaning: Failure to flush hot with solvent; lack of ultrasonic cleaning leaves orifice contamination.

● Process temperature too low: Dope solidifies prematurely in the capillary.

● Raw-material impurities: Gels, mechanical debris, undissolved particles.

● Degradation/crosslinking: Overheating or long residence causes hardened species.

● Temperature miscontrol: Too low → high viscosity; too high → charring.

● No purge at shutdown: Residual dope solidifies or scales after solvent loss.

● Filter failure: Damaged or underspecified filters allow contaminants through.

● Flow-path dead zones: Stagnant volumes cause solidification.

prev
Causes of eccentricity in hollow fiber spinning
Causes of nonuniform multi-orifice spinning
next
Related questions
no data
GET IN TOUCH WITH Us
Ready to work with us ?

About Trustech

Contact Us
Follow Us
Customer service
detect