● Not fixed—fully determined by the polymer system. It must match the processing temperature window.

● Melt spinning (e.g., PP, PE): Typically 180–300°C (PP ~200–260°C).

● Wet spinning (NIPS for PVDF/PSf): Room temperature to ~90°C; control aims at viscosity stability.

● TIPS: Most stringent; control above the polymer–diluent binodal, typically 150–250°C within a narrow window.

● Core principle: Set temperature to ensure optimal, stable rheology without thermal degradation (too high) or clogging (too low).